| 产品名称 | 粒度分布(μm) | 化学成分 (wt%) | 生产工艺 | 松装密度 | 流动性 | 喷涂工艺 | 应 用 | |||||||
| Co | C | Fe | W | Cr | B | Si | Ni | |||||||
| WC-12Co | -45+15,-63+10 | 11-13 | 5.15-5.6 | ≤ 0.8 | Bal. | 烧结破碎 | 5.5-6.5g/cm³ | ≤ 25s/50g | APS HVOF | 耐磨损,耐震动磨损 | ||||
| WC-12Co | -45+15,-38+10,-30+5 | 11-13 | 5.15-5.6 | ≤ 0.8 | Bal. | 团聚烧结 | 4.0-6.0g/cm³ | ≤ 25s/50g | APS HVOF HVAF | 通用机械,耐磨损,耐震动磨损 | ||||
| WC-12Co( 低碳 ) | -45+15, -53+20 | 11-13 | 4.0-4.4 | ≤ 0.8 | Bal. | 团聚烧结 | 4.0-6.0g/cm³ | ≤ 18s/50g | HVOF HVAF | 连续镀锌线锌浴辊 | ||||
| WC-17Co | -45+15,-38+10,-30+5 | 15.5-18 | 4.8-5.6 | ≤ 0.8 | Bal. | 团聚烧结 | 3.5-5.5g/cm³ | ≤ 25s/50g | APS HVOF HVAF | 通用机械,耐磨损,耐震动磨损,韧性好 | ||||
| WC-25Co | -45+15,-38+10 | 23.5-26 | 4.3-4.8 | ≤ 0.8 | Bal. | 团聚烧结,致密化 | 3.0-5.5g/cm³ | ≤ 25s/50g | APS 爆炸喷涂 | 耐震动磨损,韧性好 | ||||
| WC-10Ni | -45+15,-30+5 | 5-6 | ≤ 0.1 | Bal. | 9-11 | 团聚烧结 | 4.0-6.0g/cm³ | ≤ 18s/50g | ||||||
| WC-12Ni | 5-6 | 11-13 | 3.5-6.0g/cm³ | ≤ 30s/50g | ||||||||||
| WC-17Ni | 4.8-5.5 | 16-18 | 3.5-6.0g/cm³ | ≤ 30s/50g | APS HVOF HVAF | 非磁性耐磨涂层,更好的耐腐蚀性 | ||||||||
| WC-10Co4Cr | -45+15, -38+10 | 9.5-11 | 5.3-5.8 | ≤ 0.8 | Bal. | 3.5-4.5 | 烧结破碎 | 5.5-6.5g/cm³ | ≤ 25s/50g | APS HVOF HVAF | 石油、纸张、通用机械, 替代镀硬铬 | |||
| WC-10Co4Cr | -25+5,-15+5 | 9.5-11 | 5.3-5.8 | ≤ 0.8 | Bal. | 3.5-4.5 | 团聚烧结 | 3.5-5.5g/cm³ | 稳定输送至送粉器 | HVOF HVAF | ||||
| WC-20%CrC-7Ni | -45+15,-38+10,-30+5 | 5.5-8.5 | ≤ 0.8 | Bal. | 15.5-19.5 | 5.5-8.5 | 团聚烧结 | 3.0-5.0g/cm³ | ≤ 25s/50g | APS HVOF HVAF | 用于 200℃低浓度酸碱环境,750℃抗氧 化耐磨,替代性镀硬铬 | |||
| WC-42%CrC-16Ni | -45+15,-38+10,-30+5 | 6.5-8.5 | ≤ 0.8 | Bal. | 35-39.5 | 15-17 | 团聚烧结 | 3.0-5.0g/cm³ | ≤ 25s/50g | APS HVOF HVAF | 用于 200℃低浓度酸碱环境,替代镀硬铬 | |||
| WC-30WB-10Co | -45+15,-53+20,-38+10 | 9-11 | 3.5-3.9 | Bal. | 1.4-1.7 | 团聚烧结 | 3.0-4.9g/cm³ | ≤ 30s/50g | ||||||
| WC-30WB-5Co5Cr | -45+15,-53+20,-38+10 | 4-6 | 3.5-3.9 | Bal. | 4-6 | 1.4-1.7 | 团聚烧结 | 3.0-4.9g/cm³ | ≤ 30s/50g | HVOF HVAF | 用于连续镀锌线锌浴辊 | |||
| Cr3C2-20NiCr | -45+15, -53+20 | 9-11 | ≤ 0.8 | Bal. | 15-17.5 | 团聚烧结 | ≥ 2.3g/cm³ | 稳定输送至送粉器 | APS HVOF | 815℃抗氧化耐磨 | ||||
| Cr3C2-25NiCr | -45+15, -53+20 | 9-11 | ≤ 0.8 | Bal. | 19-21.5 | 团聚烧结 | ≥ 2.3g/cm³ | 稳定输送至送粉器 | APS HVOF | 815℃抗氧化耐磨 | ||||
| Cr3C2-30NiCr | -45+15, -53+20 | 8.5-10.5 | ≤ 0.8 | Bal. | 23-25.5 | 团聚烧结 | ≥ 2.3g/cm³ | 稳定输送至送粉器 | APS HVOF | 815℃抗氧化耐磨,更好的韧性 | ||||